WHIP MIX - Cristobalite Inv
Low Heat Investment
# 119630 - Mfg # 01228
Features:
* The principal ingredient, CRISTOBALITE, gives high thermal expansion, even at comparatively Low temperatures.
* It is possible to use the same creamy MIX by simple standard vacuum or painting techniques for all types of inlays.
* The usual WHIP MIX care in compounding and control assure a uniform water/powder ratio and consequent uniform expansion.
Description:
* Water/Powder Ratio:30 ml - 100 g
* Working Time: 3 minutes.
* Setting time: 16 minutes.
* Ready For Burnout: 30 minutes.
* Setting Expansion: 0.50 %
* Thermal Expansion 650 Degrees C: 1.25 %
* Compressive Strenght, Wet: 700 Psi ( 5 Mpa )
Package: 144 - 50 g